Voici toute la procédure telle qu'elle fût décrite par un certain Gary C. sur Britmodeller il y a une dizaine d'années (pardon c'est en Angliche):PEYO a écrit : sam. 18 oct. 2025 14:18 Salut,
C’est pourtant ce que je fais…mais cela ne suffit pas.
PeYo
C'est ce que fais depuis que j'ai lu ça et ça fonctionne trés bien."The best way to get all Japanese decals ( Fujimi, Hasegawa, Tamiya etc)to work as they're supposed to is use hot water and the correct setting solutions. You'll need a bottle each of Gunze Mr Setter and Mr Softer. Micro sol and others won't work as they're formulated differently. Do not use Gunze on Microscale or Cartograf decals as it will chew right through them.
Dip the decal in hot water, it doesn't need to be boiling but it does need to be fairly hot. The temperature of a drinkable tea will do. The glue is heat activated and is what makes up most of the thickness. If you dip it in cold water you'll spend the rest of the day waiting and cursing.
Lay down some Mr Setter, this is in the blue bottle. It acts as an additional glue. Slide the decal onto it and into postion and leave it alone. The decal should wrinkle a little.
Give it 10 mins or so and go over the decal with a brush with a little Mr Softer (green bottle) on it. Use sparingly as it is extremely hot. Too much and it will damage the paint, especially the weaker acrylics. The decal will now wrinkle a lot. Do not touch it as it is almost liquified at this point.
Once it is dry it will have smoothed out and will lay down beautifully over just about any raised or recessed detail you care to think of. Used properly it is probably the best conforming decal process in the industry. Used incorrectly and you'll be just another guy complaining about crap Japanese decals."
On peu aussi remplacer Mr.Setter et Mr. Softer par la solution décals de Tamiya "Mark Fit" (qui existe aussi en version Super Strong).